GlossarySolder paste
Solder paste
Solder paste is a mixture of fine solder powder and flux that is printed or jetted onto a circuit board's pads. Surface-mount parts are placed into it, and it melts into solder joints during reflow.
How it works
Paste has two parts. The metal is a powdered solder alloy, sized by a type number: a higher type means finer powder for smaller apertures. The flux is a sticky vehicle that holds the powder together, holds parts in place after placement, and cleans oxides from the metal when heated. J-STD-005 covers paste requirements, and J-STD-006 covers the alloys.
Most lines print paste through a stencil. A squeegee pushes paste across the foil, and it fills each aperture and releases onto the pad. Some high-mix lines jet paste dot by dot from a programmed pattern instead, with no stencil.
After printing, many lines check the deposits with solder paste inspection, which measures height, area and volume before any part goes down. Parts are then placed, and the board goes through reflow.
Paste is perishable. It is stored cold, brought to room temperature before use, and has a limited working life on the stencil.
Solder paste vs flux
Solder paste already contains both metal and flux. Flux alone cleans metal so solder wets, but it adds no solder. In hand soldering the solder comes from cored wire, and in wave soldering it comes from the solder pot. Rework often uses gel or liquid flux with no paste at all.
Why it matters
Too little paste opens a joint. Too much floods a fine-pitch gap into a bridge or floats a QFN off its pads. Paste that dried on the stencil or sat out too long prints poorly across the whole lot. Many surface-mount defects start at print, which is why paste volume is the first thing many lines measure.
Solder paste inspection (SPI) checks printed volume before placement, and automated optical inspection after reflow catches bridging. Each catches what the other cannot.
How to get it right
- Match the alloy to the process and the parts. Lead-free assemblies commonly use a tin, silver and copper alloy. A tin-lead build, where allowed, belongs in the assembly notes, not as a surprise on the line.
- Control the printed volume. Aperture size, stencil thickness and powder type set the volume. Fine-pitch pads and large thermal pads often need different aperture designs on the same stencil.
- Respect working life. Paste that has sat too long on the stencil or out of cold storage will not reflow the same way as fresh paste.
- Mind the finish. The surface finish on the pad changes how the paste wets when it melts.
- Store and thaw it correctly. Keep paste refrigerated as the maker specifies, let a jar reach room temperature before opening so moisture does not condense into it, and record when it came out of storage.
- Inspect the print. Solder paste inspection measures the volume, area and height of each deposit before parts are placed, which catches printing problems before they become joint defects.
Solder paste in robotics and drone hardware
Motor drivers and power stages on robot and drone boards often use QFN or power packages with a large center ground pad. A full pad of paste under that package traps gas and floats the part, lifting the signal pins off their pads. The fix is a windowed aperture that prints less paste in a pattern of smaller openings and gives gas an escape path. The same board often carries 0201 or 0402 passives that need fine powder and tight volume. One paste and one stencil have to serve both.