GlossaryReflow soldering
Reflow soldering
Reflow soldering is the process of heating a circuit board in a controlled oven so printed solder paste melts, wets the pads and component leads, and cools into solder joints. It is the main soldering step for surface-mount parts.
How it works
After solder paste is printed and parts are placed, the board rides a conveyor through a row of heated zones. Most ovens heat by forced convection. Some use vapor phase, where the board sits in the vapor of a boiling fluid that sets a fixed top temperature.
Reflow profile
The reflow profile is the temperature over time curve a board follows through the oven. It has four parts:
- Preheat. The board warms at a controlled ramp so parts and the laminate do not crack from thermal shock.
- Soak. Temperatures even out across heavy and light parts, and the flux in the paste activates and cleans the metal.
- Peak. The board goes above the alloy's liquidus, the temperature where the solder is fully molten, long enough for every joint to wet.
- Cooling. A controlled cool sets the joints and the grain structure of the solder.
Engineers build the profile by attaching thermocouples to a sample board, running it through the oven and adjusting zone settings until every measured point sits inside the paste maker's window and below each part's limit. Moisture-sensitive packages carry a peak temperature rating set by their classification under J-STD-020.
Reflow vs wave soldering
Reflow melts paste already printed on surface pads by heating the whole board. Wave soldering passes the underside of the board over a standing wave of molten solder to join through-hole leads. Many mixed boards use reflow for surface parts and then wave or selective soldering for through-hole parts.
Why it matters
If the profile runs too hot, parts, pads and laminate are damaged. If it runs too cool, or time above liquidus is too short, joints come out grainy and weak. Either way the defect repeats across the panel, because every board sees the same oven.
Profile problems also show up as specific defects. Uneven heating across a small chip part lifts one end into a tombstone. Trapped flux gas leaves voids under thermal pads. Plastic packages that took on moisture can crack or delaminate as that water turns to steam.
How to get it right
- Profile the real board. A profile set for one design does not carry over to a board with different copper weight, size or part mix.
- Give the shop the constraints. Peak temperature limits, moisture-sensitive parts and any mixed alloys belong in the assembly notes.
- Bake moisture-sensitive parts when required. Follow J-STD-033 handling for parts that exceeded their floor life.
- Inspect after the first reflow. AOI, and X-ray where joints are hidden, should follow the first board before the lot is committed.
- Keep the profile with the revision. Store the oven profile, thermocouple locations and paste type with the board revision, so a rebuild months later starts from the recipe that worked, and profile again when the board, the paste or the oven changes.
Reflow soldering in robotics and drone hardware
Robot and drone boards often mix large thermal masses with tiny parts. A motor driver board with a heavy ground pour and a big power package on one end and 0402 passives on the other can warp or tombstone if the profile is set for an average board. The heavy end needs more soak to come up to temperature. The light end needs protection from overheating while it waits. Boards with BGA processors add the need for X-ray after reflow, because a poor profile shows up under the package where no camera can see.