GlossaryDelamination
Delamination
Delamination is the separation of layers inside a printed circuit board or a component package, where the bond between laminate, prepreg, copper or mold compound fails. It shows up as blisters, bulges or internal gaps, and it breaks electrical connections, cracks plated holes and lets in moisture.
How it works
A PCB is a stack of glass-reinforced resin layers and copper foils bonded under heat and pressure. During reflow soldering, the board heats quickly. Moisture absorbed in the resin turns to steam and builds pressure between layers, while the materials expand at different rates. If the pressure and stress exceed the bond strength, layers separate. Lead-free soldering, with its higher peak temperatures, raises the stress.
Laminate materials are tested for their resistance to this. IPC-TM-650 method 2.4.24.1 measures time to delamination at a fixed high temperature using thermomechanical analysis, and laminate data sheets report it. Components suffer the same mechanism: plastic packages absorb moisture, and steam during reflow separates the die or lead frame from the mold compound, sometimes cracking the package. J-STD-020 classifies components by moisture sensitivity level, and J-STD-033 sets how to store, bake and handle them.
Delamination vs measling
Measling is the separation of glass fibers from the resin at weave intersections inside the laminate, seen as small white spots under the surface. It is a more localized condition, often judged cosmetic within limits. Delamination is a separation between layers or between laminate and copper, larger in extent, and a defect in nearly every class.
Why it matters
Delamination is often invisible from outside until it causes a failure. It cracks via barrels and inner layer connections, which produces intermittent opens that appear only when hot or under vibration. It also lowers insulation resistance and opens paths for conductive filament growth. Boards with many layers, heavy copper or multiple reflow cycles are most at risk.
How to get it right
- Specify laminates rated for lead-free assembly, with suitable glass transition temperature and decomposition temperature.
- Control moisture: store boards sealed, and bake them before assembly when exposure exceeds limits.
- Handle moisture-sensitive components according to their level, with dry storage and floor-life tracking.
- Limit reflow and rework cycles, and design so heavy parts do not need extra heat.
- Use cross-sections and thermal stress tests on new designs and suppliers.
Delamination in robotics and drone hardware
Robot and drone boards are often thick, multilayer and copper-heavy in their power sections, and they go through double-sided reflow and selective soldering. That combination raises delamination risk. Specifying laminate properties on the fab drawing, controlling board and component moisture in assembly, and qualifying with cross-sections keeps it out of fielded hardware.