Research Careers Contact

GlossaryENIG

ENIG

ENIG (electroless nickel immersion gold) is a surface finish that plates copper pads with nickel and a thin layer of gold, giving flat, solderable pads with a long shelf life. It is a common default for boards with fine-pitch parts.

How it works

ENIG is applied after solder mask, only on exposed copper. The board goes through a chemical sequence. First the copper is cleaned and activated. Then a layer of nickel is deposited by an electroless reaction, which needs no electrical connection to the pads. Last, the board goes into an immersion gold bath, where gold replaces a thin layer of nickel at the surface.

The gold protects the nickel from oxidizing. During reflow soldering, the thin gold dissolves into the molten solder and the joint forms on the nickel, as a tin-nickel intermetallic. The nickel is the real solderable surface and also acts as a barrier between the copper and the solder.

IPC-4552 is the IPC specification for ENIG plating. IPC lists Revision B as published in 2021. IPC-6012 also lists ENIG among the finishes it covers.

ENIG vs ENEPIG

ENEPIG adds a layer of electroless palladium between the nickel and the gold. The palladium protects the nickel during the gold step and gives a surface that can take gold or aluminum wire bonding as well as solder. ENIG is less expensive and is the usual choice for soldering only. ENEPIG is chosen when the board needs wire bonding or when a design wants extra margin against nickel corrosion.

Why it matters

ENIG is flat. That matters for fine-pitch QFNs, BGAs and small passives, where an uneven finish can tilt a part or leave a joint short of solder. It also keeps well in storage, so boards can wait for assembly. And it holds up through more than one reflow cycle, which double-sided builds need.

ENIG has one well-known failure mode. If the nickel corrodes during the gold step, the surface can form a dark, brittle layer that solder wets but does not bond to well. The joint looks normal and then cracks under stress. This is often called black pad. Process control at the fabricator is what prevents it, which is why IPC-4552 sets limits on the layers and their testing.

How to get it right

  • Name it on the drawing. Write "ENIG per IPC-4552" in the finish note on the fabrication drawing so the shop knows which specification applies.
  • Use it where flatness matters. If the board has fine-pitch parts, a flat surface finish is the safer choice. If every part is large, HASL is enough.
  • Do not use it for sliding contacts. Edge connectors that see repeated insertion need hard gold, as on gold fingers. ENIG's thin gold wears through.
  • Keep storage sealed. ENIG keeps well, but boards still absorb moisture. Store them in sealed bags and follow the assembler's guidance on baking older boards.
  • Ask about process control. For boards with fine-pitch parts or high-reliability joints, ask the fabricator how it monitors nickel and gold thickness against IPC-4552.
  • Watch for black pad on returns. If joints on ENIG pads fail with a dark, brittle nickel surface, send samples for cross-section analysis and share the results with the fabricator.

ENIG in robotics and drone hardware

Robot and drone boards often combine a fine-pitch processor or sensor with larger connectors and power parts. One fine-pitch part on the board is enough to set the finish for every pad, and ENIG is the common answer. Small lots built on a schedule that slips also benefit from a finish that keeps on the shelf. Boards that face vibration put more weight on joint strength, which is one more reason to buy ENIG from a fabricator with tight process control.