Wetting

Wetting is the spreading and bonding of molten solder on a metal surface. Good wetting means the solder flows out over the pad and lead, forms a smooth, concave fillet with a low contact angle and bonds to the metal through an intermetallic layer.

How it works

Molten solder only wets clean metal. Flux removes oxides from the pad and lead and keeps them from reforming during heating. Once the surfaces are clean and hot enough, tin in the solder reacts with the copper or nickel beneath and spreads. The angle the solder makes with the surface, the wetting angle, shows how well it wetted. Low angles mean good wetting.

Two failures are named. Nonwetting means the solder never bonded, and the base metal shows. Dewetting means the solder spread, then pulled back into mounds, leaving a thin film. J-STD-002 and J-STD-003 define solderability tests for component leads and board surfaces. IPC-A-610 and J-STD-001 use wetting as an acceptance criterion for every joint type.

The bond itself is an intermetallic compound, or IMC, that forms where tin reacts with the base metal. On copper, the main compounds are Cu6Sn5 and Cu3Sn. On nickel, as with ENIG, the layer is a nickel tin compound. It starts on the order of a micron thick and grows with every reflow pass, rework and long exposure to heat. No IMC means no bond. Too much IMC makes a brittle joint, since the compound is hard while bulk solder is ductile. IPC-7095 covers IMC behavior in BGA joints.

Wetting vs solderability

Solderability is a property of a surface before soldering: how readily it will wet. Wetting is what actually happens in the process. A surface with good solderability still wets poorly if the profile is too cool or the flux is spent.

Why it matters

A joint that did not wet has little strength and unstable resistance, even if it looks filled. Poor wetting is behind many defects, including cold joints, head-in-pillow and opens on hidden joints.

How to get it right

  • Store parts and boards so their finishes do not oxidize, and use them within shelf life.
  • Choose a surface finish suited to the parts and storage time.
  • Use a profile that reaches the paste's peak and time above liquidus.
  • Match flux activity to the surfaces being soldered.
  • Test solderability of suspect lots before building.
  • Limit reflow passes and rework on a joint, and cross-section qualification builds to check IMC thickness.

Wetting in robotics and drone hardware

Robotics programs often stock parts and boards for months between small builds. Finishes and leads age in storage, and wetting suffers. Tracking storage time and testing old stock before a build avoids weak joints on boards that vibrate in use. Drones crash and robots take impacts, and brittle IMC layers are where joints crack under shock, especially on BGAs.