Pin-in-paste, also called intrusive reflow, is a way to solder through-hole components in the same reflow oven as surface-mount parts. Solder paste is printed into and around the plated holes, the through-hole parts are inserted through the paste, and reflow melts the paste to form the joints, removing a separate wave or selective soldering step.

How it works

The stencil prints paste over each through-hole pad and into the hole. When a pin is pushed through, it carries some paste into the barrel. During reflow, the paste melts, flows down the barrel by capillary action and forms fillets on both sides of the board.

The hard part is volume. Solder paste is roughly half metal by volume, so the printed paste has to be about twice the volume of the finished joint: the barrel minus the pin, plus top and bottom fillets. An IPC technical paper on through-hole connector assembly explains that this volume is often more than a normal print delivers, so designs use overprinting, where the stencil aperture extends beyond the pad onto the solder mask, thicker or stepped stencils, or solder preforms placed alongside the paste to add metal.

Components must survive reflow temperatures. Many through-hole connectors and parts use plastics rated only for wave soldering, so parts for pin-in-paste need bodies rated for the full reflow profile, and often standoffs so they do not sit in the paste.

Pin-in-paste vs wave soldering

Wave soldering passes the board over a wave of molten solder to solder through-hole parts after surface-mount reflow. It handles any number of through-hole joints with plenty of solder, but needs a separate machine, fixtures or pallets to protect bottom-side parts, and adds a process step. Pin-in-paste does everything in one reflow pass, but only works when the parts tolerate reflow and enough paste fits.

Why it matters

Many boards are almost entirely surface mount but keep a few through-hole connectors for strength. Pin-in-paste lets those boards skip wave or selective soldering, which cuts cost, handling and cycle time. Done wrong, it leaves voids and thin fillets that fail inspection.

How to get it right

  • Calculate the required paste volume for each pin from hole, pin and fillet geometry.
  • Size holes close to the pin, since every bit of extra barrel volume needs more paste.
  • Use overprint, a stepped stencil or preforms when a normal print is short, following IPC-7525 stencil guidance.
  • Specify parts rated for reflow temperatures, with standoffs.
  • Inspect hole fill and fillets against J-STD-001 requirements on first builds.