GlossaryTin whiskers
Tin whiskers
Tin whiskers are thin, hair-like crystals of tin that grow spontaneously from tin-plated surfaces, such as component leads, terminals and connector contacts. They grow over months or years without heat or current, and a whisker long enough to touch a neighboring conductor causes a short circuit.
How it works
Pure tin finishes develop compressive stress, from plating conditions, from intermetallic compounds forming between tin and copper underneath, from mechanical loading and from temperature cycling. Tin relieves that stress by extruding whiskers. They are electrically conductive, and NASA's whisker research catalogs failures they caused in satellites, medical devices and other equipment.
A whisker that bridges two conductors at low current carries it and causes an intermittent or permanent short. At higher current it melts open, which makes the fault hard to find afterward. In vacuum, it vaporizes into a conductive plasma arc. Whiskers also break loose and lodge elsewhere in an assembly.
Tin-lead solder and finishes resist whisker growth. When lead was removed from most electronics, pure tin finishes became common again, and the risk returned. JEDEC JESD201 sets environmental acceptance tests for tin finishes, and JESD22-A121 gives the method for measuring whisker growth.
Tin whiskers vs dendrites
Dendrites are metal growths that form across a board surface from electrochemical migration, when moisture, contamination and voltage are present. Tin whiskers need none of those: they grow from internal stress in the tin itself, and they grow outward from the surface. Cleaning and coating prevent dendrites, while whisker mitigation focuses on the finish and its stress.
Why it matters
Products with long service lives, fine-pitch parts and high reliability needs are most exposed, since whiskers take years to grow and short narrow gaps. The failures are intermittent and appear in the field long after qualification. For robots and drones expected to run for years in varying temperatures, whiskers are a slow risk that design choices control.
How to get it right
- Specify finishes with whisker mitigation, such as matte tin over a nickel barrier or annealed tin.
- Ask suppliers for whisker test data against JESD201 for parts in critical areas.
- Use conformal coating, which slows whiskers and blocks many from reaching neighbors.
- Avoid mechanical stress on tin-plated contacts, such as press-fit pins and clamped terminals, where possible.
- Investigate intermittent shorts in fielded units with whiskers in mind.
Tin whiskers in robotics and drone hardware
Connectors, fine-pitch processors and power components on robot and drone boards often have tin finishes. Thermal cycling outdoors and vibration add stress. Conformal coating on controller boards, careful finish selection for connectors, and supplier data on critical parts are the usual controls. Whisker risk is one reason high-reliability buyers ask about finishes on the BOM.